介绍缅甸达贡山镍矿冶炼高品位镍铁的工艺改进和生产实践。通过取消石灰石熔剂的配入、将镍品位由25%提高到35%、焙砂温度提高到700℃以上、强化系统原料控制等措施,有效解决了电炉长期存在的泡沫渣和翻料等工艺问题,产能达到设计产能108%以上,各项消耗指标大幅下降。
Abstract:Technical improvement and plant practice of production of high grade Ni-Fe alloy from nickel laterite in Myanmar Dagaung Taung were introduced.With measures including canceling limestone addition,improving nickel grade from 25% to 35%,raising calcine temperature to 700 ℃ above,and strengthening raw material control etc,long term technical problem of foaming slag in electric furnace is solved effectively,production capacity is 108% of the designed capacity,and consumption index drops sharply.
[1]赵景富.RKEF工艺处理缅甸镍红土矿[J].有色金属(冶炼部分),2013(1):8-10.
[2]杨涛,李小明,赵俊学,等.红土镍矿处理工艺现状及研究进展[J].有色金属(冶炼部分),2015(6):9-13.
[3]黄希祜.钢铁冶金原理[M].2版.北京:冶金工业出版社,1990:165-168.
[4]王亚琴.红土镍矿深度还原—磁选工艺的分析研究[D].沈阳:东北大学,2011.
[5]宋丹娜,王雪琴.我国镍铁产业发展现状及趋势研究[J].四川有色金属,2015(1):5-9.
[6]陈树江,田凤仁.相图分析及应运[M].北京:冶金工业出版社,2007:231-235.
基本信息:
中图分类号:TF644
引用信息:
[1]罗红卫,姬鹤志,杨利忠.红土矿生产高品位镍铁的工艺改进和生产实践[J].有色金属(冶炼部分),2017(08):16-19+29.
2017-08-12
2017-08-12