| 275 | 9 | 22 |
| 下载次数 | 被引频次 | 阅读次数 |
铝电解槽的电能消耗量与平均电压和电流效率两个因素有关,降低槽电压或者提高电流效率,可降低铝电解槽直流电耗。通过系统测试系列电解槽电压平衡、能量平衡、电流效率,深入挖掘分析,提出了节能降耗技术措施。通过2台试验槽工业试验表明,试验槽平均电压3.819 V,电流效率92.89%,吨铝直流电耗12 251 kWh。与系列电解槽相比,平均电压降低99 mV,电流效率提高1个百分点,吨铝直流电耗降低455 kWh,节能效果显著。
Abstract:The electrical energy consumption of aluminum electrolysis cells is related to two factors: average voltage and current efficiency.Reducing the cell voltage or improving current efficiency can reduce the DC power consumption of aluminum electrolysis cells.Through systematic test of voltage balance, energy balance and current efficiency of a series of electrolytic cell, and in-depth analysis, the technical measures of energy saving and consumption reduction were put forward.The industrial test of two test tanks shows that the average voltage of the test tank is 3.819 V,the current efficiency is 92.89%,and the DC power consumption per ton of aluminum is 12 251 kWh.Compared with the series electrolytic cell, the average voltage is reduced by 99 mV,the current efficiency is increased by 1 percentage point, the DC power consumption per ton of aluminum is reduced by 455 kWh, and the energy saving effect is remarkable.
[1] FENG N X,TIAN Y F,PENG J P,et al.New cathodes in aluminum reduction cells[J].Light Metals,2010:405-408.
[2] 赵应彬,王平,陈谦.300 kA新式异型阴极双钢棒铝电解槽生产实践[J].有色金属(冶炼部分),2014(2):28-30.ZHAO Y B,WANG P,CHEN Q.Plant practice of 300 kA double steel bars aluminium electrolysis cell with new shaped cathode[J].Nonferrous Metals (Extractive Metallurgy),2014 (2):28-30.
[3] 张亚楠,柴登鹏,史志荣,等.新型稳流保温铝电解槽节能技术的工业推广应用[J].有色金属(冶炼部分),2018(7):21-24.ZHANG Y N,CHAI D P,SHI Z R,et al.Industrial application of energy-saving technology based on steady flow and heat preservation[J].Nonferrous Metals (Extractive Metallurgy),2018(7):21-24.
[4] MAHRAN G M A,ALI M M.Numerical simulation of cathodic voltage drop in Hall-Héroult cell[J].Minerals Engineering,2020,157:106534.DOI:10.1016/j.mineng.2020.106534.
[5] PARIDA D R,SINGH R,KALO N,et al.Effect of using a copper insert on stability and energy balance in an aluminum production cell[J].The Indian Institute of Metals,2021,74(2):487-498.
[6] 焦庆国,侯光辉,张旭贵,等.燃气焙烧启动技术在石墨化阴极电解槽的工业应用与分析[J].有色金属(冶炼部分),2023(2):29-33.JIAO Q G,HOU G H,ZHANG X G,et al.Industrial application and analysis of gas roasting starting technology in aluminum electrolysis cell with graphitized cathode[J].Nonferrous Metals (Extractive Metallurgy),2023(2):29-33.
[7] 张刚刚,沈贵元,李喜元,等.500 kA大型铝电解槽生产管理实践[J].轻金属,2022(2):22-28.ZHANG G G,SHEN G Y,LI X Y,et al.Production management practice of 500 kA large-amperage aluminum pot[J].Light Metals,2022(2):22-28.
[8] 汤伟,刘雅锋.500 kA铝电解槽阴极节能技术升级与应用[J].轻金属,2022(5):28-33.TANG W,LIU Y F.Upgrading and application of cathode energy-saving technology for 500 kA aluminum reduction cells[J].Light Metals,2022(5):28-33.
[9] 李贺松,李庆贺,李晓东.铝电解槽几种节能阴极电-热场耦合仿真研究[J].轻金属,2019(4):31-38.LI H S,LI Q H,LI X D.Research on electrothermal field coupling simulation of several energy-saving cathodes in aluminum reduction pots[J].Light Metals,2019(4):31-38.
[10] 邱竹贤.预焙槽炼铝[M].北京:冶金工业出版社,2005.QIU Z X.Aluminum smelting in prebaked cells[M].Beijing:Metallurgical Industry Press,2005.
[11] 汪艳芳,张旭贵,李健,等.低阻高性能阳极钢爪材料开发设计及工业试验[J].有色金属(冶炼部分),2021(11):46-53.WANG Y F,ZHANG X G,LI J,et al.Development and industrial test of low resistance and high performance anode steel claw material[J].Nonferrous Metals (Extractive Metallurgy),2021(11):46-53.
基本信息:
中图分类号:TF821
引用信息:
[1]张阳,张亚楠,方斌,等.铝电解槽节能潜力分析与应用实践[J].有色金属(冶炼部分),2023(08):43-49.
基金信息:
2021年中国铝业股份有限公司科技研发项目(中铝股份科发字[2021]214号)
2023-07-14
2023-07-14